(a) Monomer conversion vs time curve and corresponding ln[M0]/[M] plot and (b) evolution of number-average molecular weight (Mn) and dispersity (Mw/Mn) with conversion for the RAFT aqueous dispersion polymerization of DAAM at 70 °C and pH 2.5 using a DDMAT-PDMAC58 macro-CTA targeting DDMAT–PDMAC58–PDAAM120. Conditions: 20% w/w solids and a macro-CTA/AIBN molar ratio of 10.