Skip to main content
. 2017 Nov 21;19(5):1435–1444. doi: 10.1021/acs.biomac.7b01403

Figure 4.

Figure 4

DSC heating curves for solutions of block copolymers HO-PEtOx-b-PIPOx (A) and HO-PIPOx-b-PEtOx (C) and dispersions of block copolymer-grafted SPION FeOx@PEtOx-b-PIPOx (B) and FeOx@PIPOx-b-PEtOx (D) in Milli-Q-water, concentration of 1 mg mL–1, heating rate 1 K min–1, 20 to 90 °C, curves normalized on MW of the individual PIPOx-blocks.