Published in final edited form as: Biomaterials. 2006 Jun 14;27(29):5039–5048. doi: 10.1016/j.biomaterials.2006.05.034

Fig. 8.

Fig. 8.

Salicylate-based polymer resists degradation and induces a limited foreign-body response. Area of initial polymer implantation is identified (*) in inactive control (A) and salicylate-based (B) polymer. Skin and capsule collagen stains blue and muscle tissue appears red. Higher-power images from the center of the implant indicate the degradation of the polymer (*) and invasion of cells (arrows) in inactive polymer (C) and salicylate-based polymer (D). Original magnification 100 × (A, B) and 400 × (C, D).