Physiochemical characteristics of the CA/EDTA-stabilized cerium oxide nanoparticle (CeNP) series.

Citric Acid/EDTA Ratio Size in Solution DLS (nm) Polydispersity Crystallite Size via XRD (nm) Zeta Potential (mV)
100/0 7.8 0.374 2.0 −20.8
70/30 3.8 0.309 2.3 −20.4
60/40 2.6 0.198 2.4 −18.7
50/50 2.7 0.188 2.4 −21.5
40/60 2.9 0.162 2.5 −18.3
30/70 3.0 0.188 2.5 −23.0
20/80 3.5 0.160 2.4 −9.1
0/100 2.4 0.230 2.1 −15.70