Table 3.

Experimental plan and experimental results after 7 cycles of homogenization in the microfluidizer.

run P (MPa) PPI (%) COR (-) D[4,3] (nm) D[3,2] (nm) Span
1 60 50 2 1215 ± 32 145.0 ± 0.1 3.91 ± 0.09
2 150 50 2 575 ± 27 115.0 ± 0.1 1.2 ± 0.1
3 60 90 2 1178 ± 104 139.0 ± 0.6 3.2 ± 0.5
4 150 90 2 343 ± 35 111.3 ± 0.6 1.85 ± 0.03
5 60 50 4 453 ± 57 114.3 ± 0.5 2.3 ± 0.2
6 150 50 4 222 ± 12 109.3 ± 2.3 1.26 ± 0.06
7 60 90 4 860 ± 65 118.2 ± 0.1 6.0 ± 0.2
8 150 90 4 212 ± 19 109.3 ± 0.5 1.58 ± 0.04
9 60 70 3 654 ± 6 123.0 ± 0.2 2.6 ± 0.1
10 150 70 3 227 ± 10 106.7 ± 2.3 1.6 ± 0.1
11 105 50 3 210 ± 2 112.7 ± 0.6 1.12 ± 0.05
12 105 90 3 252 ± 6 110.0 ± 0.3 1.69 ± 0.01
13 105 70 2 375 ± 18 116.7 ± 0.6 1.15 ± 0.01
14 105 70 4 297 ± 9 109.0 ± 0.1 1.78 ± 0.04
15 105 70 3 268 ± 12 111.0 ± 2.0 2.19 ± 0.09
16 105 70 3 255 ± 4 110.8 ± 0.1 1.73 ± 0.01
17 105 70 3 279 ± 15 112.1 ± 0.2 1.81 ± 0.01
18 105 70 3 250 ± 9 110.3 ± 0.6 1.72 ± 0.02