Skip to main content
. 2021 Jan 14;13(1):99. doi: 10.3390/pharmaceutics13010099

Figure 2.

Figure 2

Characterization of nanoparticles. (A) Particle size, (B) PDI, (C) particle size and (D) PDI change in 7 days at room temperature of PTR-701Ns and RPTR-701Ns. Data were presented as the mean ± SD (n = 3).