Skip to main content
. 2021 Oct 18;22(11):4633–4641. doi: 10.1021/acs.biomac.1c00927

Figure 5.

Figure 5

Coassembly of BTA-OEG4 with different polysaccharides in water. (a) UV–vis spectra of BTA-OEG4 in water (500 μM) coassembled with Acetyl-HA, HA 700 kDa, AA, dextran, and HA 10 kDa at a 2:2 weight ratio. (b) Strain sweep oscillatory rheology at 37 °C (fixed angular frequency of 1 rad/s) of BTA-OEG4 in water (2 wt %) alone or coassembled with Acetyl-HA, HA-700 k, and dextran (1 wt %).