Z-average after 8 h of milling with different stabilizer solutions. Composition is given in % (w/w) and HPC-SL concentration was kept constant at 0.9%. Milling was carried out at 4 °C with 1500 rpm and milling beads sized 0.3–0.4 mm. Hatched area: No stable nanosuspension was obtained. Values are given as mean of three measurements.