Skip to main content
. 2022 Nov 28;8(12):776. doi: 10.3390/gels8120776

Figure 3.

Figure 3

Figure 3

Frequency sweep of the formulations: (a) HA-Dop formulations, (b) BB formulations. N = 3. At an oscillation frequency of 1 Hz, all the gels have similar rheological properties; however, with increasing frequency, HA-Dop-based formulations remain stable throughout the sweep, while BB gels elastic modulus increases.