Particle size distribution (PSD) of raw and agglomerated PPSPs with different concentrations of MD binder.

Sample MD
Concentration
(%)
D10 (μm) D50 (μm) D90 (μm) Span
Raw PPSP   17.2 ± 0.01 f 64.8 ± 0.07 e 165 ± 1.39 f 2.28 ± 0.02 a
Agglomerated PPSP 0 (control) 133 ± 3.00 a 311 ± 7.93 a 637 ± 12.5 a 1.62 ± 0.01 c
10 80.0 ± 0.91 e 191 ± 1.08 c 395 ± 3.35 b 1.66 ± 0.02 b
20 104 ± 1.57 c 195 ± 3.52 c 331 ± 4.07 d 1.17 ± 0.02 d
30 116 ± 0.59 b 234 ± 1.21 b 380 ± 1.14 c 1.13 ± 0.00 e
40 88.4 ± 1.30 d 179 ± 1.39 d 300 ± 1.89 e 1.18 ± 0.01 d

Each value is the mean of triplicate measurements ± SD. Means with different lowercase letters (a–f) within each column are significantly different (p < 0.05).